Skip to main content
. 2014 Sep 22;7(9):6853–6864. doi: 10.3390/ma7096853

Table 4.

Board densities are given as a function of lingo-cellulose nanofibers (LCNF) content.

Samples Density (g/cm3) Standard Deviation
WF (control) 0.97 0.02
WF:LCNF = 95:5 0.97 0.03
WF:LCNF = 90:10 0.99 0.02
WF:LCNF = 85:15 0.97 0.03

WF: wood flour.