Skip to main content
. 2014 Aug 7;7(8):5711–5734. doi: 10.3390/ma7085711

Figure 9.

Figure 9

SEM of aluminum alloy AA6061 surface after exposure for 30 days in acidic solution (a) without PIL and (b) with 100 mg·L−1 of PImC12.