. 2014 Aug 7;7(8):5711–5734. doi: 10.3390/ma7085711

Figure 10.

Figure 10

SEM image of a cross-section of the aluminum alloy AA6061 surface after exposure for 30 days in the acidic solution (a) without PILs and (b) with 100 mg·L−1 of PImC12.