. 2014 Aug 5;7(8):5633–5642. doi: 10.3390/ma7085633

Figure 6.

Figure 6

Example for a typical Al2O3 AD layer on an alumina substrate after deposition. Deposition parameters: 100% O2, film thickness t ≈ 8 µm.