Skip to main content
. 2016 Jan 14;9(1):50. doi: 10.3390/ma9010050

Table 1.

Dispersive component of the surface energy (γsd), acid (Ka) and base (Kb) constants and acid/base ratio (Ka/Kb) of the cellulose nanofibrils (CNF) and alginate films at 25 °C.

Sample γsd (mJ/m2) * Ka Kb Ka/Kb
CNF 39.79 0.08 0.20 0.4
Alginate 38.66 0.09 0.05 1.8
Alginate with 10 wt % CNF 36.87 0.09 0.04 2.3

* Correlation coefficient between 0.998 and 0.999.