Skip to main content
. 2004 Apr 27;2004(1):24–34. doi: 10.1155/S1110724304306017

Table 2.

Osteogenic differentiation of hMSC plated on indicated substrates for 16 days, as assessed by indicated measurements of mineral to matrix ratio. By comparison, fully differentiated osteoblasts cultured on tissue culture plastic for 21 days have a ratio of approximately 5.4.

HMSC plated on substrate/medium Mineral to matrix ratio

Tissue culture plastic/DMEM 1.662
Tissue culture plastic/OS 1.515
Collagen I/DMEM 1.763
Collagen I/OS 2.372
Vitronectin/DMEM 2.767
Vitronectin/OS 2.761