Figure 4.

Figure 4

LIPSS fabricated on copper surfaces with (ac) different laser fluences F at fixed pulse number N = 509 and (df) with different number of pulses N at F = 0.43 J/cm2. Reprinted from Long et al. [49], Copyright 2014, with permission from Elsevier.