Skip to main content
. 2016 Jun 30;9(7):535. doi: 10.3390/ma9070535

Figure 2.

Figure 2

Appearance of FA geopolymer after thermal treatment: (a) flushing of FA paste specimens after heating to 1000 °C; and (b) transverse cracks on FA paste specimens after heating to 600 °C.