. 2016 Jun 30;9(7):535. doi: 10.3390/ma9070535

Figure 3.

Figure 3

Residual compressive strengths of metakaolin (a) and fly ash (b) geopolymer pastes and mortars after exposure to high temperatures. Standard deviations are depicted as error bars.