. 2016 Jul 20;9(7):596. doi: 10.3390/ma9070596

Figure 8.

Figure 8

SEM images of the fractured surfaces after tensile test. (a) CS; (b) ML; (c) SLM; and (d) ML/PS (500×, scale bar = 30 μm).