Surface roughness values of different groups measured by AFM. No significant changes were observed in Ra, Rz or Rms values after UV treatment of zirconia samples.

Sample Ra (µm) Rms (µm) Rz (µm)
Control UV Control UV Control UV
Zr1-m 0.12 (±0.02) 0.09 (±0.02) 0.17 (±0.03) 0.13 (±0.02) 1.04 (±0.21) 0.76 (±0.09)
Zr1-r 0.21 (±0.08) 0.29 (±0.07) 0.29 (±0.07) 0.36 (±0.08) 1.3 (±0.18) 1.39 (±0.2)
Zr2-m 0.03 (±0.01) 0.03 (±0.01) 0.04 (±0.01) 0.04 (±0.01) 0.20 (±0.02) 0.19 (±0.03)
Zr2-r 0.31 (±0.11) 0.27 (±0.03) 0.38 (±0.13) 0.34 (±0.04) 1.67 (±0.26) 1.53 (±0.11)