(a) Size measurements of the NPs resulting from LA of an Au target, from both DLS of the colloidal solution and analysis of TEM image after drop-casting on silicon substrate; (b) UV-vis absorption of the colloidal solution; (c) TEM image showing the size of the NPs in the direct space; (d) XRD pattern resulting from a sample of drop-cast Au NPs.