PCM Number of the Cycle Melting Onset Point (°C) Freezing Onset Point (°C) Melting Latent Heat (J/g) Freezing Latent Heat (J/g)
TD-LA/EP-5 wt % AP 0 cycle 24.5 25.4 77.78 79.02
1000 cycles 24.9 25 75.63 77.89
2000 cycles 25.1 24.7 74.39 75.92