Skip to main content
. 2017 Apr 28;10(5):466. doi: 10.3390/ma10050466

Figure 14.

Figure 14

Scanning electron micrographs of Fe- (a) and Ti-contaminated (b) ZTA surfaces after an in vitro hydrothermal cycle of 200 h. Corresponding CL spectra are shown in (c,d), respectively, as collected at the spots depicted in the insets to each micrograph.