Skip to main content
. 2017 May 8;10(5):516. doi: 10.3390/ma10050516

Table 1.

Sample preparation conditions of CSCaP composites and thermogravimetric analysis.

Sample CS/CaP Weight Ratio Theoretical Mineral Content, % Humidity at 55 °C, % 1 Residual Weight at 650 °C, % 1
CSCaP1 56:3.75 6.25 8.9 7.3
CSCaP2 56:14 20.0 9.0 19.4
CSCaP3 56:26.3 31.9 8.0 20.3

1 As determined by thermogravimetric analysis of the samples.