(A) Picture of the crucibles taken out of the furnace and left to crystallize on a sheet of stainless steel. The left crucible shows a sample of pure salt (white) (60/40 ratio–NaNO3/KNO3) whilst the next three samples (left to right) contain increasing concentrations of copper oxide calculated to be 0.32, 0.98 and 1.65 wt. %; (B) Top view of 0.98 wt. % CuO samples; (C) View of the underside of 0.98 wt. % CuO solid salt mixture.