Table 1.

Groups of the different treated Y-TZP surface in the present study.

Groups Surface Treatment & Condition (37 °C) Groups Surface Treatment & Condition (Thermal Cycling: 5–55 °C)
P Polishing PT Polishing
A 110 μm A12O3 Blasting AT 110 μm A12O3 Blasting
AS 110 μm A12O3 Blasting + Silane Primer AST 110 μm A12O3 Blasting + Silane Primer
AM 110 μm A12O3 Blasting + MDP Primer AMT 110 μm A12O3 Blasting + MDP Primer
AMS 110 μm A12O3 Blasting + MDP Containing Silane Primer AMST 110 μm A12O3 Blasting + MDP Containing Silane Primer