Table 1.

Mean (standard deviation) of repassivation times (Tre; ms) from the last scratching cycle for both commercially pure titanium (CP-Ti) and titanium alloys containing 20 mass% chromium (Ti-20Cr) at different scratching speeds.

Specimens Scratching Speed
10 mm/s 20 mm/s 40 mm/s
Commercially pure titanium (CP-Ti) 312 (31) a,A 152 (23) b,A 108 (26) b,A
Titanium alloys containing 20 mass% chromium (Ti-20Cr) 378 (19) a,B 173 (33) b,A 80 (13) c,A

Results of statistical analysis are represented by lower and upper case letters. Different lowercase letters in the same column indicate that the groups are significantly different (p < 0.05). Different upper case letters in the same row indicate that the groups are significantly different (p < 0.05).