Sample ML=−μB<LZ> MS=−g0μB<SZ> ML/MS
Co monolayer θ=0° 0.39±0.03 μB 1.19±0.08 μB 0.33±0.11 μB
Co monolayer θ=45° 0.44±0.03 μB 1.39±0.08 μB 0.28±0.11 μB
Ni monolayer θ=0° 0.35±0.02 μB 1.39±0.12 μB 0.25±0.14 μB
Ni monolayer θ=45° 0.34±0.02 μB 1.50±0.12 μB 0.23±0.14 μB
Co thick film θ=45° 0.44±0.03 μB 1.25±0.08 μB 0.36±0.11 μB
Ni thick film θ=45° 0.17±0.02 μB 1.34±0.12 μB 0.13±0.14 μB