Figure 1

First cycle voltage profiles during galvanostatic cycling at a C/30 rate (1C = 1675 mA gs–1): (a) at 30 °C using bulk sulfur electrode in ACN–TTE compared to bulk sulfur electrode in DOL:DME and (b) at 55 °C using bulk sulfur electrodes in ACN–TTE compared with DOL:DME; specific discharge and charge capacities over multiple cycles for bulk sulfur electrodes in ACN−TTE compared to DOL:DME; (c) at 30 °C and (d) 55 °C. The DOL:DME electrolyte contains 2 wt % LiNO3 additive.