Fig. (12).

Fig. (12)

(A) Schematic illustrating the preparation of electrospun PEO/PLLA/OA-Fe3O4 nanofibers. (B) SEM image of PEO/PLLA/OA-Fe3O4 nanofibers with 20% OA-Fe3O4 loading. The scale bar is 20 μm. (C) Time-dependent temperature curves of the magnetoactive membranes at different concentrations of Fe3O4 at 110 kHz and 25 mT magnetic field. (D) Cumulative percentage release profiles of acetaminophen from PEO/PLLA/acetaminophen fiber samples containing 0, 20, and 70 % OA-Fe3O4. (Reprinted from ref. [162])