Figure 3. Room- and cryogenic-temperature tensile properties.

Figure 3

Room- and cryogenic-temperature engineering stress–strain curves of the H750 and H900 alloys. At cryogenic temperatures, the strengths and elongation are improved over the room-temperature values. Higher yield and tensile strengths and lower elongation are shown in the H750 alloy. (The data points shown are the mean±s.d. from 3 repeated measurements).