Skip to main content
. 2016 Mar 23;9(4):216. doi: 10.3390/ma9040216

Figure 5.

Figure 5

SEM micrographs of rapid laser-melted Mg-xMn alloys after immersion in SBF at 37 °C for 48 h: (a) pure Mg; (b) Mg-1Mn, area A was covered with integrated protective film, while area B presented relatively shallow cracks; (c) Mg-2Mn; (d) Mg-3Mn.