Skip to main content
. 2016 Mar 25;9(4):234. doi: 10.3390/ma9040234

Figure 9.

Figure 9

(a) The shear stress-strain curves for a given crosslink density of 17.3% at different temperatures; and (b) the broken ratio versus temperature.