Table 1.
Specimen | Carbon Content (wt %) |
---|---|
Elemental powder mixture(Al-Mg-Sn) | 0.22 ± 0.52 |
Final powder mixture with 20 wt % PMMA | 11.29 ± 0.52 |
Final powder mixture with 25 wt % PMMA | 12.17 ± 0.43 |
Final powder mixture with 30 wt % PMMA | 13.03 ± 0.61 |
Sintered porous Al with 20 wt % PMMA | 3.87 ± 0.54 |
Sintered porous Al with 25 wt % PMMA | 0.41 ± 0.15 |
Sintered porous Al with 30 wt % PMMA | 0.43 ± 0.16 |