Figure 5

XRD patterns of samples (a) 90.48 wt % A/9.52 wt % S; (b) 84.57 wt % A/15.43 wt % S; (c) 13.60 wt % A/86.40 wt % S; and (d) 7.69 wt % A/92.31 wt % S. All of them heated at 1350 °C. (S: silicocarnotitess, A: Nurse’s A-phasess; R: (α-C2S-α′TCP)ss).