Skip to main content
. 2017 Mar 16;10(3):305. doi: 10.3390/ma10030305

Figure 2.

Figure 2

SEM image of the Cu powder with the magnifying power of 1 kx (a); the Cu powder with the magnifying power of 9 kx (b); cross section of the green body (c); surface of the sintered part with heating rate (3 °C/min), highest temperature (1083 °C), holding time (3 h) (d).