Skip to main content
. 2017 Mar 16;10(3):305. doi: 10.3390/ma10030305

Figure 8.

Figure 8

Green samples printed by a novel additive manufacturing method with: (a) the temperature of the substrate 30 °C; (b) the temperature of the substrate 50 °C; (c) the temperature of the substrate 70 °C; (d) the temperature of the substrate 90 °C.