Skip to main content
. 2017 Mar 16;10(3):305. doi: 10.3390/ma10030305

Figure 12.

Figure 12

Energy dispersive X-ray (EDX) analysis of the sintered sample with heating rate (3 °C/min), highest temperature (1083 °C), and holding time (3 h).