Potentiodynamic scans in 10% H2SO4 at 25 °C of Fe-40Cr alloy in comparison to an alloy where Cr is partially substituted by Al (Fe-35Cr-5Al) and the other two alloys where both are modified by micro-addition of Ru (0.2%) (reprinted from [75] with permission of Elsevier).