. 2017 Mar 9;10(3):272. doi: 10.3390/ma10030272

Figure 3.

Figure 3

(a) TEM; (b) SAED; and (c) HRTEM images of 20 h milled Fe–10Cr–3Al powder. Edge dislocations are observed in the inverse fast Fourier transform (FFT) image (inset).