Skip to main content
. Author manuscript; available in PMC: 2018 Jan 1.
Published in final edited form as: Acta Biomater. 2016 Oct 6;47:91–99. doi: 10.1016/j.actbio.2016.10.008

Figure 7.

Figure 7

A) Representative image of the appearance of a dry, crimped composite (left) and a saturated composite (right). Scale bar is in centimeters. B) Volume expansion ratio and shape recovery analysis of the wound dressing composite that incorporates the PEG 6 kDa 5wt% hydrogel and H40 SMP foam after submersion in RO water at 37°C, (mean ± standard deviation, n = 5).