Skip to main content
. 2016 Jul 28;9(8):627. doi: 10.3390/ma9080627

Figure 2.

Figure 2

Schematic outline of sintering parameters employed during sintering run for Mg-0.3Ca alloy specimens indicating stage I—vacuum heating, stage II—sintering and stage III—cooling. The sample temperature is less than the set furnace temperature because of the temperature deviation in the furnace.