Figure 4.
Intersection between the Gibbs energies of -Fe (blue) and α-Fe (yellow) at K while gradually distorting the α-Fe lattice from its equilibrium state (0% α-Fe lattice distortion) to the maximum distortion given by Equation (6) (100% α-Fe lattice distortion). The lattice parameter of the -Fe phase is kept constant at its equilibrium value for every composition (see Equation (4)).