Scanning electron microscopy (SEM) images of 500-µm-wide channels with 50 × 50 µm2 Ag dots. (a,b) Top view of Ag dots before recovery; (c,d) Top and side view of the sample after recovery; (e,f) Close-up of the vertical sidewall with the broken Ag dots and ripples.