Skip to main content
. 2013 Mar 15;6(3):1028–1049. doi: 10.3390/ma6031028

Figure 2.

Figure 2

Discharge cell voltage vs. gravimetric capacity of the Li//LNMCO cells for various C-rate for (a) the as-grown cathode material and (b) heat treated sample with sucrose at 600 °C for 30 min in air. (Reprinted with permission from [57]. Copyright 2011 Elsevier.)