Figure 9.

Figure 9

Modified Peukert plot of the Li//C-LiFePO4-coated and uncoated LiMn1.5Ni0.5O4 cells between 3.0 and 4.9 V. (Reprinted with permission from [66]. Copyright 2012 Elsevier.)