FIGURE 1.

FIGURE 1

Hydrolysis of siRNA-loaded polyplexes in aqueous solution. A: 1H-NMR analysis reveals HDG polymer hydrolysis at 24 and 48 h (arrows indicate either the appearance or disappearance of peaks over time due to hydrolysis). B: Structure of hydrolyzed HDG polymer (top) and quantification of polymer hydrolysis at 24 and 48 h (bottom). C: HDG-NPs (right) reduced in size after 24 h, indicating hydrolytically dependent nucleic acid release.