Skip to main content
. 2017 Jul 20;7:6017. doi: 10.1038/s41598-017-06115-0

Figure 10.

Figure 10

(a) SEM image at x120 of fracture surface from Al2O3 bar obtained by sintering boehmite printed with DIW. Fracture resulted from Three-point bending test. Stacked lines are not discernible in the center of the sample, but clearly visible on the samples surface. (b) SEM image at x10000 of the same fracture surface. The object is dense with a fine grained microstructure, suitable for high strength mechanical properties