. 2017 Jul 5;8:1375–1387. doi: 10.3762/bjnano.8.139

Figure 5.

Figure 5

AFM topography characteristics considering a 1 × 1 μm2 area, after deposition of [Ni2L(HL5)](ClO4) (7) on gold with an rms roughness of 13 Å.