Table S2.
Average ± SEM | P value | |||||
Condition | 30 kPa | 60 kPa | Glass | 30 kPa vs. 60 kPa | 60 kPa vs. glass | 30 kPa vs. glass |
Collagen–spread area | 1048 ± 72 | 2013 ± 124 | 2515 ± 127 | 0.002 | 0.03 | 0.0004 |
Collagen–aspect ratio | 2.07 ± 0.15 | 1.57 ± 0.07 | 1.49 ± 0.07 | 0.04 | n.s. | 0.02 |
Collagen–circularity | 0.50 ± 0.03 | 0.64 ± 0.02 | 0.61 ± 0.03 | 0.009 | n.s. | 0.03 |
Ecad-Fc–spread area | 929 ± 28 | 1550 ± 48 | 2039 ± 128 | 0.0003 | 0.02 | 0.0001 |
Ecad-Fc–aspect ratio | 2.62 ± 0.019 | 1.49 ± 0.02 | 1.46 ± 0.06 | 1.39E-06 | n.s. | 6.80E-05 |
Ecad-Fc–circularity | 0.39 ± 0.03 | 0.59 ± 0.03 | 0.72 ± 0.03 | 0.009 | 0.02 | 0.0009 |
Shown is analysis corresponding with the data presented in Fig. 1. Values presented are averages and SEM calculated from three independent experiments. Statistics were determined using a Student’s t test.