Table 1.
The effect of different preparation methods on physicochemical properties of blank PCL and mePEG-PCL nanoparticles (n = 3 ± SD).
| Mean diameter ± SD (nm) | PDI ± SD | Zeta potential ± SD (mV) | ||
| PCL nanoparticles | nanoprecipitation | 168 ± 3 | 0.10 ± 0.02 | −17 ± 0.4 |
| emulsification/solvent evaporation | 184 ± 3 | 0.29 ± 0.4 | −18 ± 0.8 | |
| double emulsion | 352 ± 2 | 0.39 ± 0.02 | −8 ± 0.1 | |
| mePEG-PCL nanoparticles | nanoprecipitation | 77 ± 3 | 0.17 ± 0.04 | −13 ± 3.2 |
| emulsification/solvent evaporation | 146 ± 3 | 0.27 ± 0.004 | −19 ± 1.3 | |
| double emulsion | 170 ± 2 | 0.19 ± 0.01 | −5 ± 0.24 | |