Table 1. Surface roughness measurements of the various samples, showing an increased average surface roughness with increasing cross-linker density.

Sample Average surface roughness (Å) Dispersity (±%)
Chitosan 4588 250
Chi-TEOS IPN 6347 200
Chi-TEOS IPN-Ag 9174 209
Chi-TEOS IPN-Au 9722 196