Skip to main content
. 2017 Aug 1;7:6972. doi: 10.1038/s41598-017-07086-y

Figure 8.

Figure 8

TEM images and selected area electron diffraction patterns of the 75Li2S-25P2S5 sulfide glass ceramic. (a,b) Bright-field images before annealing and after annealing at 180 °C. (c,d) Selected area electron diffraction patterns taken from the bright-field images.