SEM images of example fracture surfaces - (a) macrograph of z-575, (b) crack initiation from a pore, (c) striations in the crack growth region, (d) SEM image of the fast fracture over-load region; (e) macrograph of z-760. (f) Crack initiation from a smooth facet, and (g) crack initiation from two conjoined gas pores.