Scanning electron microscopy (SEM) photographs of BNBC10T6 samples obtained by solid state method. Powder synthesized at (a) 800 °C for 4 h and corresponding ceramics prepared by low temperature sintering at (b) 970 °C; (c) 990 °C and (d) 1000 °C for 5 h. Powder synthesized at (e) 800 °C for 1 h and corresponding ceramics prepared by high temperature sintering at (f) 1020 °C; (g) 1050 °C and (h) 1080 °C for 1 h.