Skip to main content
. 2017 Jul 4;10(7):748. doi: 10.3390/ma10070748

Figure 11.

Figure 11

Polarization photomicrographs of the final morphologies of (a,b) neat PLA and (c,d) PLAC (PLA-graphene composite) after melt crystallization (120 °C); The scale bars are (a,c) 50 and (b,d) 20 μm [65].