Skip to main content
. 2017 Jul 14;10(7):796. doi: 10.3390/ma10070796

Figure 4.

Figure 4

Polarization plots for the 3D-printed GDL [80% PA + 20% Ti] used membrane and electrode assembly (MEA) and normal MEA tested with humidified H2/O2 at 75 °C and 15 psi pressure.