Processing parameters for laser cladding and isothermal transformation.

Laser Cladding Isothermal Heat Treatment
Laser Power (W) Preheating Temperature (°C) Scanning Velocity (mm/s) Powder Feed Rate (g/min) Isothermal Temperature (°C) Isothermal Times (h)
2500 220 10 30 200 1, 2, 4, 8, 12, 24, 48,
2400 270 10 30 250 1/2, 1, 2, 3, 4, 8, 12, 16
2300 320 10 30 300 1/4, 1/2, 3/4, 1, 3/2, 2, 3, 4, 6
2200 370 10 30 350 1/4, 1/3, 1/2, 3/4, 1, 1.5, 2, 3, 4