Figure 7.

Figure 7

The enamel demineralization tested by transverse microradiography (TMR). (a) Mineral volume content of the enamel bonding with composites by QAM adhesives; (b) mineral loss (n = 6); and (c) lesion depth (n = 6) of enamel bonding with composites by adhesives containing QAMs with different alkyl chain lengths (CL = 3, 6, 9, 12, and 16) or none. Bars with the same letter indicate a value having no significant distance, and those with different letters indicate a significant difference (p < 0.05).